Picture 23 Soak - 1 Fired as follow : 100° P/H to 600°  then 150° P/H to Temp 1186° Soak 15Min ..

--------------

Fired Nick

25 Oct 2025

100 ° P/H to 600 ° Soak 45 Min

150 ° P/H to 1050 ° Soak 15 Min

90 ° P/H to 1175 ° Dan Afkoel

----------------------------------------
New Fire
Segment 1: 100° P/H to 600° Soak 45  Min
Segment 2: 150° P/H to 1000° No Soak
Segment 3: 70° P/H to 1172° Soak 25 Min

  • Keep the kiln closed until it naturally cools to about 850 °C.
    That’s roughly 1 hour 30 minutes after the program ends on a full kiln.

  • Then you can crack open the peephole slightly for airflow down to 700 °C.
    This mimics a 60 °C/hr controlled descent.



  • (23) - GCS738

    • Brand: GlazeCore
    • Product Code: GCS738
    • Availability: In Stock
    • R0.00